I have used wheel weights for casting in the past, and I just got it really
hot (in well ventilated area) and skimmed off the garbage on the surface.
--
** FREE Fishing Lures
** Weekly drawing
** Public Fishing and Boating Forums
**
www.YumaBassMan.com
"JWirth4702" wrote in message
...
I have found that when adding recycled (scrap) lead to my melting pot that
a
higher temp is needed to keep it melted. Also the top third of the melted
metal
is 'slushy'.
Is there a way to add good lead and mix the two back to a workable metal?
Is
there an additive that can be used for the same (tin, bismuth, flux???)
Jay Wirth
Renaissance Ink
1613 Rita Rd
Vestal, NY 13850
www.renaissanceink.net
607 748 4665