I have used wheel weights for casting in the past, and I just got it really
hot (in well ventilated area) and skimmed off the garbage on the surface.

--
** FREE Fishing Lures
** Weekly drawing
** Public Fishing and Boating Forums
** www.YumaBassMan.com


"JWirth4702" wrote in message
...
I have found that when adding recycled (scrap) lead to my melting pot that

a
higher temp is needed to keep it melted. Also the top third of the melted

metal
is 'slushy'.

Is there a way to add good lead and mix the two back to a workable metal?

Is
there an additive that can be used for the same (tin, bismuth, flux???)
Jay Wirth